  1. Vor 20 Stunden · and a lower peel adhesion with copper foil. All of the copper−coated films exhibited an increase in peel adhesion as the PDMS content increased. The adhesion strength between PI–copper foil films without PDMS doping was the worst, while the adhesion strength between PI–copper foil films increased as PDMS doping increased. PI-1/3% and PI-2/3%